Precautions for use:
1. Clean the tile floor before use to keep the floor free of dirty water stains. If the gap between the tiles is too deep, use a sealant to fill the gap first. The product does not need to be mixed and can be brushed immediately after opening the lid. Before construction, block the floor drain to prevent glue leakage.
2. For large-area construction, it is recommended to first wall and then the floor,
3. It is recommended that the place be ventilated after construction. The colloid should not be exposed to water or stepped on before it is dry and solidified. When the colloid is at room temperature above 20°C, it will dry in 2 hours and can form a film in 5 hours. The lower the temperature, the slower the curing (lower temperatures in winter will cure Time may affect).